Conductive PPS
Conductive PPS Polymers
How to improve the conductivity of polyphenylene sulfide?
1. Blending and copolymerization:
Blending or copolymerizing PPS with other conductive polymers (such as polyaniline, polypyrrole, etc.) can improve its conductive properties.
2. Composite materials:
Preparing PPS-based composite materials, such as PPS/conductive filler composite materials, PPS/conductive polymer composite materials, etc., can improve conductivity.
What are the applications of conductive polyphenylene sulfide?
1.Manufacture of electronic components, switches, relays and other parts that require electrical conductivity.
2.Electrodes for fuel cells
Product name: Conductive polyphenylene sulfide
Conductive PPS Material characteristics:
Conductive, high temperature resistance, flame retardant, high flow
Typical Data Sheet:
ITEM(23℃) |
METHOD |
UNIT |
Test Data |
Physical and chemical properties |
|||
Density |
ISO 1183 |
g/cm³ |
1.68 |
Water absorption |
ISO 62 |
% |
0.02 |
Molding shrinkage (level) |
ISO 294-4 |
% |
0.2 |
Molding shrinkage (vertical) |
ISO 294-4 |
% |
0.8 |
Flammability rating |
UL-94 |
Class |
V-0 |
Mechanical properties |
|||
Tensile Strength |
ISO 527 |
MPa |
150 |
Elongation at break |
ISO 527 |
% |
1.5 |
Bending strength |
ISO 178 |
MPa |
240 |
Flexural modulus |
ISO 178 |
GPa |
12 |
Lzod notch impact |
ISO 180 |
kJ/m² |
6 |
Thermal properties |
|||
HDT(1.80MPa) |
ISO 75 |
℃ |
270 |
MI |
ISO 1133 |
g/10min |
90 |
Electrical properties |
|||
Surface resistivity |
IEC 60093 |
Ω·m |
103 |
Injection molding process |
|||
Pre-drying |
Temperature |
℃ |
120-140 |
Time |
h |
4-6 |
|
Mold temperature |
130-150℃ |
Barrel temperature |
Front temperature |
Processing temp |
Rear temperature |
290-310℃ |
290-310℃ |
280-300℃ |
Features: conductive, high temperature resistance, flame retardant, high flow
Usage: battery cover, anti-static clamp, electronic tray, etc.
If you want to know the price of polyphenylene sulfide, you can send a quotation request by email.